Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 22.76 MPa | 3301 psi | JIS-K-6723 |
Denka REOMER G G3012 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |