Mechanical Properties Metric English Comments
Tensile Strength at Break 21.9 MPa
3170 psi
50 mm/min. Type IV; ASTM D638
LyondellBasell Alathon® M5372 High Density Polyethylene
ApplicationsALATHON M 5372 copolymer with narrow weight distribution. This resin provides high impact strength and stress crack resistance, excellent color, low odor and good processing stability. ..
Tensile Strength at Break 21.9 MPa
3170 psi
ASTM D3759
3M Scotch® 8654 Cold Temperature Reinforced Strapping Tape
Scotch® Cold Temperature Reinforced Strapping Tape 8654 is a high performance, transparent packaging tape. This tape is reinforced along its length with continuous poly propylene monofilaments, whi..