Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.184 MPa | 316.8 psi | Air at 158°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |