Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 21.4 MPa | 3110 psi | Cross Direction; ASTM D3756 |
3M 7260M High Temperature Over Spray Protective Bags and Sheets 3M™ High Temperature Over Spray Protective Bags and Sheets 7260M are used for masking where high temperature resistance or custom sizes are needed. This high performance product is designed for mas.. |