Mechanical Properties Metric English Comments
Tensile Strength at Break 307 MPa
44500 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA
LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.