Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1310 - 2100 MPa | 190000 - 305000 psi | |
Goodfellow Tungsten 75/Rhenium 25 Alloy When used with Tungsten the alloy is an important high temperature thermocouple wire. The alloy can also be used as a filament.Information provided by Goodfellow. |