Mechanical Properties Metric English Comments
Tensile Strength at Break 30.6 MPa
4440 psi
ASTM D882-83A (mod)
Lord Adhesives 320 / 322 Epoxy Adhesive
LORD® 320/322 adhesive is a general purpose, two component epoxy adhesive system formulated for primerless adhesion to automotive sheet molded compounds (SMC). This adhesive system also provides ..