Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 20.50 - 30.50 MPa | 2973 - 4423 psi | ZCI-T-008 |
Zeon Chemicals Zetpol® 1020 Hydrogenated Nitrile Elastomomer Zeptol 1020 is a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance o.. |