Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.90 MPa | 566 psi | ISO 37 |
PolyOne OnFlex™ S KG 70A-3S2019 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Strength at Break | 3.90 MPa @Temperature 23.0 °C |
566 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE) Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Strength at Break | 3.90 MPa @Temperature 23.0 °C |
566 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE) Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Tensile Strength at Break | 3.90 MPa | 566 psi | ASTM D412 |
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Tensile Strength at Break | 3.90 MPa | 566 psi | Across Flow; ASTM D412 and ISO 37 |
ExxonMobil Santoprene® 121-60M200 Thermoplastic Vulcanizate - UV Resistant Product Description: A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated with high flow properties and excellent aesthet.. |