Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.48 MPa @Time 7200 sec |
505 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7057-1000 TPE Product Description: StarMediflex P 7057-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tensile Strength at Break | 3.48 MPa | 505 psi | |
Abatron AboSeal 8104-14 Polysulfide, Thixotropic Sealant and Caulk AboSeal 8104-14 is a 2-part, 100% solids, thixotropic polysulfide. It only comes in black. It is great for expansion joints on floors and decks with heavy traffic. It is a structural, heavy-duty sta.. |