Polymer Property : Tensile Strength at Break = 3.35 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.35 MPa

@Time 7200 sec
486 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-55-1000 TPE
Product Description: StarXTRUDE XTR-55-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P..