Mechanical Properties Metric English Comments
Tensile Strength at Break 3.01 MPa

@Temperature 23.0 °C
437 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7736-1 Thermoplastic Elastomer (TPE)
Dynaflex™ G7736-1 is a general purpose compound designed to provide easy processing and a good surface finish. - Good Aesthetics - Good Ozone/UV Stability - High Flow for Thin-Wall Parts - Overmold..