Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.05 MPa | 297 psi | Heat Cycle - 6 cycles of 4 hrs @ 121°C, 40 mins @ 160°C, and 1 hr @ 182°C |
3M AC-730 Class B-12 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Tensile Strength at Break | 2.05 MPa | 297 psi | Heat Cycle - 6 cycles of 4 hrs @ 121°C, 40 mins @ 160°C, and 1 hr @ 182°C |
3M AC-730 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Tensile Strength at Break | 2.05 MPa | 297 psi | Heat Cycle - 6 cycles of 4 hrs @ 121°C, 40 mins @ 160°C, and 1 hr @ 182°C |
3M AC-730 Class B-6 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Tensile Strength at Break | 2.05 MPa | 297 psi | Heat Cycle - 6 cycles of 4 hrs @ 121°C, 40 mins @ 160°C, and 1 hr @ 182°C |
3M AC-730 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |