Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 293 MPa | 42500 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RC008 PA 66 LNP THERMOCOMP* RC008 is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength at Break | 293 MPa | 42500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |