Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 20.1 MPa | 2920 psi | ASTM D1414, ASTM D412 |
DuPont Performance Polymers Kalrez® AeroSeal™ 7800 Fluoroelastomer Kalrez AeroSeal™ 7800* perfluoroelastomer parts are a specialty black product that meets the requirements of Aerospace Material Specification (AMS) 7257. It offers outstanding thermal stability and.. |
|||
Tensile Strength at Break | 20.1 MPa | 2920 psi | |
Asahi Glass Fluon® PB3060 60% Bronze, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |