Polymer Property : Tensile Strength at Break = 289 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.99 MPa
289 psi
ASTM D412-83
3M E-FIS Fire Barrier Expantrol Flexible Intumescent Strip
3M Fire Barrier E-FIS has been designed to seal the air space between doors and frames and for glazing fire resistant glass to help prevent the passage of smoke and flames in the event of a fire. Wh..