Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 287 MPa | 41600 psi | ASTM D638 |
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Tensile Strength at Break | 287 MPa | 41600 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP UC006H PPA LNP THERMOCOMP* UC006H is a compound based on Polyphthalamide resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |