Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.8 MPa
4180 psi
ASTM D3756
3M 2214 Paper Masking Tape
3M™ Paper Tape 2214 is a general purpose paper masking tape for holding, bundling, sealing and non-critical maskingInformation provided by 3M