Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 275.0 MPa | 39880 psi | Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D638 |
Fibre Glast RAE 2426 / 2177 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |