Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 18.72 MPa @Temperature 136 °C, Time 605000 sec |
>= 2715 psi @Temperature 277 °F, Time 168 hour |
IEC 60811-1-2 |
LG Chemical LUTENE XL8080UC PE Compound Description: LUTENE XL8080UC is a superior cleanliness version for high voltage power cable insulation and is designated as UC (Ultra-Clean) due to its extremely low level of contamination. LUTENE X.. |