Polymer Property : Tensile Strength at Break = 27.46 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.46 MPa
3983 psi
Taiwan PU Corporation TPU-BTB85 Breathable Grade, Blow Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), Breathable Grade, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation.