Polymer Property : Tensile Strength at Break = 265 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.83 MPa

@Temperature 49.0 °C,
Time 173000 sec
265 psi

@Temperature 120 °F,
Time 48.0 hour
3M AC-770 Class B-1 Aerospace Sealant
3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio..
Tensile Strength at Break 1.83 MPa

@Temperature 49.0 °C,
Time 173000 sec
265 psi

@Temperature 120 °F,
Time 48.0 hour
3M AC-770 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-770 Class B are fast cure, low density two-component, manganese dioxide cure, polysulfide fuselage sealants. 3M AC-770 Class B Sealants have outstanding resistance to aviatio..