Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.0859 MPa @Temperature 85.0 °C, Time 605000 sec |
2623.14 psi @Temperature 185 °F, Time 168 hour |
Heat Aging; ISO 188, Method B |
S&E Specialty Polymers TufTech™ SE11-019D PVC Compound Application: Automotive – 90A PVC, integral colored, exterior weatherable, extrusion & injection molding compound.Information provided by S&E Specialty Polymers |