Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.0 MPa | 2460 psi | ASTM D638 |
Teknor Apex APEX® 6500-80 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 17.0 MPa | 2460 psi | ASTM D638 |
Teknor Apex APEX® 65011 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |