Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.3 MPa
3530 psi
ASTM D638
Teknor Apex APEX® 60003 Polyvinyl Chloride, Flexible
Notes: 75°C Insulation; RoHS Compliant Features: Flame Retardant Uses: Communication Wire Insulation Forms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC Article 770; NEC Article ..