Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 23.75 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.75 MPa

@Temperature 200 °C,
Time 1.21e+6 sec
3444 psi

@Temperature 392 °F,
Time 336 hour
After Dry Heat Aging; ASTM D865
Seals Eastern 7182E Fluorocarbon-Elastomer
Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc.
Copyright © lookpolymers.com All Rights Reserved