Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 23.61 MPa | 3425 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer With its broad chemical resistance, Chemraz® 555, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. Chemraz 555 provides a significantly wider operational band.. |
|||
Tensile Strength at Break | 23.61 MPa | 3425 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 551 Perfluoroelastomer With its broad chemical resistance, Chemraz® 551 is ideally suited as a universal sealing material for aqueous semiconductor wafer processing and chemical/DI water distribution systems. Chemraz .. |