Mechanical Properties Metric English Comments
Tensile Strength at Break 23.54 MPa
3414 psi
Taiwan PU Corporation TPU-C85 General Grade, Calender Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation.