Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 23.06 MPa @Temperature 100 °C, Time 3.60e+6 sec |
3345 psi @Temperature 212 °F, Time 1000 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 7202 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |