Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 15.3 MPa | 2220 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R293AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 15.3 MPa | 2220 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R295AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 15.3 MPa | 2220 psi | ASTM D638 |
LyondellBasell Integrateâ„¢ NE542013 Functionalized Polyolefin INTEGRATE products are chemically modified polyolefins used to combine dissimilar materials for a variety of applications including molding articles, flexible materials and fiber technology or to pr.. |
|||
Tensile Strength at Break | 15.3 MPa | 2220 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 95 A.01 black TPE-S, Shore A95, black TPE-SInformation provided by BARLOG plastics GmbH. |