Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 15.2 MPa | 2210 psi | ASTM D412 |
Teknor Apex Telcar® TL-81-D920-A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 15.2 MPa | 2210 psi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FT 2350 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FT 2350 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |