Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 22.9 MPa | 3320 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2195G Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2195G is a 95 Shore A non-phthalate, gamma-stable flexible vinyl compound made from FDA sanctioned ingredients. HC 2195G can be used for extrusion and injection molding healthcare applicatio.. |
|||
Tensile Strength at Break | 22.9 MPa | 3320 psi | ASTM D1414 |
Greene Tweed FLUORAZ® 888 Fluoroelastomer, FEPM Fluoraz® 888 polytetrafluoroethylene/propylene (FEPM) performs well in aggressive chemicals where ultra pure materials are not required. Recommended for conventional wet and dry system applicatio.. |
|||
Tensile Strength at Break | 22.9 MPa | 3320 psi | ISO R 527 |
Stir SpA T 91 ATC (PVC) Application: Extrusion different profilesInformation provided by STIR SpA |