Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 217 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 217 MPa

@Temperature -40.0 °C
31500 psi

@Temperature -40.0 °F
ISO 527-2
PolyOne OnForce™ LFT NN-40LGF/000 HS UV Black Polyamide 66 (Nylon 66)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Tensile Strength at Break 217 MPa
31500 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Thermocomp LC008 PEEK (Europe-Africa-Middle East)
LNP* Thermocomp* LC008 is a compound based on Polyetheretherketone resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Tensile Strength at Break 217 MPa
31500 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF009H PA 66
LNP* THERMOCOMP* RF009H is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added feature of this material is: Healthcare.
Tensile Strength at Break 217 MPa
31500 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF009H PA 66 (Asia Pacific)
LNP* Thermocomp* RF009H is a compound based on Nylon 66 resin containing Glass Fiber.