Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.1 MPa | 2050 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A8000 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R100AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | ASTM D1414 |
Greene Tweed Fluoroelastomer 742 FKM Fluoroelastomer 742 performs well in aggressive chemicals and where ultrapure materials are not required. Recommended for conventional wet and dry system applications, Fluoroelastomer 742 has a goo.. |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | ASTM D638 |
Teknor Apex APEX® 155 Polyvinyl Chloride, Flexible Notes: 80°C Jacket; RoHS CompliantFeatures: Sunlight Resistant (720 hours); Good UV Resistance Uses: Building Wire Jacketing; Wire and Cable Applications Agency Ratings: UL QMTT2 .E73402Forms: Pe.. |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | ASTM D638 |
Teknor Apex APEX® 65007 Polyvinyl Chloride, Flexible Notes: 90°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | ASTM D412 |
Teknor Apex Monprene® MP-1956A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | ASTM D412 |
Teknor Apex Monprene® MP-2327R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | ISO 37 |
Alliance Polymers Viprene™ G40D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 14.1 MPa | 2050 psi | ISO 37 |
Alliance Polymers Viprene™ G40D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G40D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |