Mechanical Properties Metric English Comments
Tensile Strength at Break 13.868 MPa
2011.4 psi
Air at 212°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 281-87MED Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad..