Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 20.75 MPa | 3010 psi | ASTM D412 |
DuPont Performance Polymers Kalrez® 8900 Fluoroelastomer DuPont™ Kalrez® 8900 perfluoroelastomer parts are a black product for all thermal processes, e.g., oxidation, diffusion furnace, metal CVD, ALD and LPCVD. It offers outstanding thermal stability, .. |