Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 20.6 MPa @Thickness 2.00 mm |
2990 psi @Thickness 0.0787 in |
50mm/min; ASTM D638 |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Tensile Strength at Break | 20.6 MPa | 2990 psi | ISO R 527 |
Stir SpA CT 89 ATC R (PVC) Application: Insert with maximum transparencyInformation provided by STIR SpA |
|||
Tensile Strength at Break | 20.6 MPa | 2990 psi | 50 microns film; ASTM D882 |
Arkema Group Orevac® 9309 Film EVA-MAH Terpolymer EVA Terpolymers based Main Application: Cast film coextrusionInformation provided by Arkema Group |
|||
Tensile Strength at Break | 20.6 MPa | 2980 psi | ASTM D3756 |
3M 256 Colored Paper Tape 3M™ Colored Paper Tape 256 can be used for masking, bundling, holding and splicing operations needing colors for identification.Information provided by 3M |