Mechanical Properties Metric English Comments
Tensile Strength at Break 20.3 MPa
2940 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Wire & Cable 1604-xx07FRD Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Tensile Strength at Break 20.3 MPa
2940 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible F70E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 20.3 MPa
2940 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible F77E Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 20.3 MPa
2940 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible SL9994 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 20.3 MPa
2940 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R276AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength at Break 20.3 MPa
2940 psi
AVG; ASTM D412 Method A
Seals Eastern 7075 Ethylene-Propylene Rubber
General service EPDM.Information provided by Seals Eastern, Inc.
Tensile Strength at Break 20.3 MPa
2950 psi
ASTM D638
Teknor Apex APEX® 65010 Polyvinyl Chloride, Flexible
Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 20.3 MPa
2950 psi
ASTM D412
Teknor Apex Monprene® MP-1991B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Tensile Strength at Break 20.3 MPa
2950 psi
ASTM D412
Teknor Apex Telcar® TL-2596C Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 20.3 MPa
2950 psi
ASTM D3756
3M 8979 Performance Plus Duct Tape
3M™ Performance Plus Duct Tape 8979 has a unique product construction for indoor and outdoor applications. This tape is removable with little or no adhesive residue from most opaque surfaces up to ..
Tensile Strength at Break 20.3 MPa
2950 psi
ASTM D3756
3M 8979N Performance Plus Duct Tape Nuclear Grade
3M™ Performance Plus Duct Tape 8979N has a unique product construction for indoor and outdoor applications. This tape is removable with little or no adhesive residue from most opaque surfaces up to..