Polymer Property : Tensile Strength at Break = 2.867 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 2.867 MPa
415.8 psi
Air at 212°F, 168 hr; ASTM D573
ExxonMobil Santoprene® 191-55PA Thermoplastic Elastomer  (discontinued **)
A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft ..