Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.404 MPa | 348.6 psi | Air at 275°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 191-55PA Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft .. |