Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 13.60 MPa | 1973 psi | ASTM D412 |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |