Tensile Strength at Break 19.9 MPa
2890 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer  (discontinued **)
A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi..
Tensile Strength at Break 19.9 MPa
2890 psi
Across Flow; ASTM D412
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character..
Tensile Strength at Break 19.9 MPa
2880 psi
ASTM D412
Teknor Apex MF 141 Polyvinyl Chloride, Flexible Film
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company
Tensile Strength at Break 19.9 MPa
2880 psi
ASTM D3759
3M Scotch® 8915 Filament Tape
Scotch® Filament Tape 8915 is a high-performance transparent tape reinforced with continuous high strength glass filaments which is designed to hold appliance parts together during manufacture and ..
Tensile Strength at Break 19.9 MPa
2880 psi
ASTM D3759
3M Scotch® 8916 Filament Tape
Scotch® Filament Tape 8916 is a high-performance transparent tape reinforced with continuous high strength glass filaments which is designed to hold appliance parts together during manufacture and ..
Tensile Strength at Break 19.9 MPa
2880 psi
ASTM D3759
3M Scotch® 897 Filament Tape
Scotch® Tape 897 is a glass-filament-reinforced tape suitable for light to medium duty strapping, bundling, reinforced applications. Scotch® Tape 897 has a synthetic rubber resin adhesive with goo..