Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 19.61 MPa | >= 2844 psi | R-350A |
Zeon Chemicals Zetpol® 2010H Hydrogenated Nitrile Elastomomer Zetpol 2010H is a high-Mooney version of a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressi.. |
|||
Tensile Strength at Break | 19.61 - 39.22 MPa | 2844 - 5688 psi | R-350A |
Zeon Chemicals Zetpol® PBZ-123 Hydrogenated Nitrile Elastomomer PBZ-123 is a polyblend of hydrogenated nitrile polymer, Zetpol 1020, and polyvinyl chloride, Nippon Zeon 101EP. This material is mechanically fluxed to create a unique polyblend which exhibits good.. |