Polymer Property : Tensile Strength at Break = 1885 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.00 MPa
1885 psi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4190 Thermoplastic Elastomer
A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4190 is a medium hardness grade possessing exceptional tensile strength, superior compression set, chemical..
Tensile Strength at Break 13.00 MPa
1885 psi
Die C; Flow direction; ASTM D412
Teknor Apex Sarlink® 4490 Thermoplastic Elastomer
A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4490 is a medium hardness grade possessing exceptional tensile strength, superior compressio..