Mechanical Properties Metric English Comments
Tensile Strength at Break 126.4 MPa
18330 psi
ASTM D3759
3M 398FR Glass Cloth Tape
3M™ Glass Cloth Tape 398FR has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typically used for se..
Tensile Strength at Break 126.4 MPa
18330 psi
ASTM D3759
3M 398FRP Printed Version Glass Cloth Tape
3M™ Glass Cloth Tape 398FRP has an acrylic adhesive for many applications requiring high adhesion, an abrasion-resistant backing and flame retardant properties. This product is typically used for s..