Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.6 - 12.5 MPa | 1540 - 1810 psi | |
3M 3635-100 Light Enhancement Film A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other.. |