Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 12.37 MPa | 1794 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 644 Perfluoroelastomer Specifically developed to meet the demands of aggressive dry plasma systems and the corresponding remote O2 cleaning processes, Chemraz® 644, a perfluoroelastomer with a unique formulation, provi.. |