Tensile Strength at Break 12.26 MPa
1778 psi
Shin-Etsu Silicones KE-167U Low Temperature Silicone Elastomer
ShinEtsu KE167U is a phenyl (PVMQ) silicone compound. This product is designed for good low temperature characteristics.Product Features: A broad range of service temperatures from 100 to +260°C ..