Mechanical Properties Metric English Comments
Tensile Strength at Break >= 11.88 MPa
>= 1723 psi
ASTM D412 Method A
Seals Eastern 7282 Neoprene / Chloroprene
UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc.