Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1170 MPa | 170000 psi | Hard |
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std All values may vary dependent on specific design and usageAlumel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsulatedPlatedInformation provided by Californ.. |
|||
Tensile Strength at Break | 1172 MPa | 170000 psi | |
Special Metals INCOLOY® alloy 908 INCOLOY® alloy 908 (UNS N09908) is an age-hardenable nickel-iron alloy which exhibits a low coefficient of thermal expansion, high tensile strength, high fracture and impact toughness, fatigue cr.. |